ʻO 321 kahi titanium stabilized austenitic chromium-nickel stainless steel i hoʻomohala ʻia e hāʻawi i kahi 18-8 type alloy me ka hoʻomaikaʻi ʻana i ka intergranular-corrosion resistance. nā hiʻohiʻona mau ma nā palena ʻai.Pono e noʻonoʻo ʻia ka 321 no nā noi e koi ana i ka hoʻomehana ʻana ma waena o 8009F (427°C) a me 1650°F (899°C)
Alloy | % | Ni | Cr | Fe | N | C | Mn | Si | S | P | Ti |
321 | Min. | 9 | 17 | kaulike | 5*(C+N) | ||||||
Max. | 12 | 19 | 0.1 | 0.08 | 2.0 | 0.75 | 0.03 | 0.045 | 0.70 |
Denstiylbm/i^3 | Coefficient oHoʻonui wela (min/in)-°F | ʻO ka hoʻoili welaBTU/hr-ft-°F | Wela KūikawāBTU/lbm -°F | Nā Module o ka Elasticity(annealed)^2-psi | |
---|---|---|---|---|---|
ma 68 °F | ma 68 – 212°F | ma 68 – 1832°F | ma 200°F | ma 32 – 212°F | i loko o ka pilikia (E) |
0.286 | 9.2 | 20.5 | 9.3 | 0.12 | 28 x 10^6 |
Papa | Ikaika U'i ksi | Ka ikaika hua 0.2% Offset ksi | ka hooloihi ana - % i loko 50 mm | ʻoʻoleʻa (Brinell) |
---|---|---|---|---|
321 | ≥75 | ≥30 | ≥40 | ≤217 |
•Kūleʻa ka oxidation a hiki i 1600°F
•Hoʻopaʻa kūʻē i ka weld wela i hoʻopili ʻia (HAZ) intergranular corrosion
•Kū'ē ka polythionic acid stress corrosion pohā
•Nā ʻenekini piston mokulele
•Nā hui hoʻonui
•Ka hana ʻana i nā pū
•Nā mea hoʻoheheʻe wela
•Mea hana hoʻoheheʻe
•Kiʻekiʻe wela kaʻina hana kemika