ʻO Hayness 188 (Alloy 188) he pahu hoʻoheheʻe cobalt-base maikaʻi loa me ka ikaika kiʻekiʻe kiʻekiʻe a me ke kūpaʻa oxidation maikaʻi i 2000°F (1093°C).ʻO ka pae chromium kiʻekiʻe i hui pū ʻia me nā mea hoʻohui liʻiliʻi o ka lanthanum e hana i kahi unahi ikaika a pale.Loaʻa i ka alloy ke kūpaʻa sulfidation maikaʻi a me ke kūpaʻa metallurgical maikaʻi loa e like me ka hōʻike ʻana e kona ductility maikaʻi ma hope o ka lōʻihi o ka ʻike ʻana i nā mahana kiʻekiʻe.Hoʻohui maikaʻi ʻia ka mea hana a me ka weldability e hoʻohana pono i ka alloy i nā noi turbine gas e like me nā combustors, nā mea paʻa ahi, nā laina a me nā ala hoʻololi.
C | Cr | Ni | Fe | W | La | Co | B | Mn | Si |
0.05 0.15 | 20.0 24.0 | 20.0 24.0 | ≦ 3.0 | 13.0 16.0 | 0.02 0.12 | bal | ≦ 0.015 | ≦ 1.25 | 0.2 0.5 |
ʻO ka mānoanoa (g/cm3) | Lae hehee (℃) | Hiki wela kiko (J/kg·℃) | Koefficient hoʻonui wela ((21-93 ℃)/℃ ) | ʻAiʻa uila (Ω·cm) |
9.14 | 1300-1330 | 405 | 11.9×10E-6 | 102×10E-6 |
Hikiwawe (pa, lapaʻau wela maʻamau)
Ka wela hoao ℃ | Ka ikaika tensile MPa | Hua ikaika (0.2hua hua)MPa | ʻO ka lōʻihi % |
20 | 963 | 446 | 55 |
AMS 5608, AMS 5772,
Bar/Rod | Uea | Hoʻopaʻa / ʻāwili | Pepa/Pula |
AMS 5608 | AMS 5772 |
•ʻO ka ikaika a me ka oxidation kū i ka 2000°F
•ʻO ka ductility ma hope o ka wā kahiko
•Kū'ē i ka sulfate waiho wela wela
ʻO nā kini puhi puhi ʻenekini kinoea, nā kī kī, nā mea paʻa ahi a me ka liner afterburner